As showed you upper bonding and crocking test report this Monday as attached pictures.
*Bonding test: utopa material have no problem but surface of 1.2mm,RAY HIDE PLUS(B2L)+JR was delaminated.
*Crocking test: standard is 100 circles but only 72 circles surface of Utopa material as below.